Related Categories:Steel Sheets
the demisions and tolerence of roofing sheet 1.Finishing length: 5mm 2.Thickness for material: 0.03mm 3.Rib heigh:25mm

AVAILABLE THICKNESS

  

Base Metal

Thickness

(mm)

Total Coated

Thickness

(mm)

Weight

(kg/m2)

Steel

Grade

Min. Yield

Strength

(MPa)

0.35

0.40

3.46

AS1397

G550

0.42

0.48

4.20

AS1397

G550

0.48

0.55

4.76

AS1397

G550

  

other thicknesses are subject upon stock availability and time delivery

RECOMMENED MAXIMUM ROOF LENGTH (M)

 

Slope in Degree

Rainfall (mm/h)

 

 

 

150

50

60

80

200

39

50

60

250

30

40

48

300

26

30

40

RECOMMENDED MAXIMUM SPACING OF SUPPORT

 

Base Metal

Thickness

(mm)

Total Coated

Thickness

(mm)

ROOFS  

WALLS

End Span

(mm)

Internal Span

(mm)

End Span

(mm)

Internal Span

(mm)

0.35

0.40

900

1000

1200

1500

0.42

0.48

1200

1500

1700

2000

0.48

0.55

1300

1700

2000

2300

INSTALLATION METHOD

It is strongly recommended that sheets are laid with the side laps facing away from the direction of the prevailing wind. Where possible, the roof sheets should be fixed with the side laps facing away from the normal line of sight.

SIDE LAP AND FLASING Side lap fasteners are required at mid spans for purlin spacings over 1,000mm and for girt spacings over 1,200mm. For all side lap and flashing fastening, use no. 10 x 25mm self drilling Hexagon Head Screw with pre-assembled neoprene bonded steel washer.

END LAPS AP RIB is available in continuous length limited only by the maximum transportable length of 20m. For longer length, end lap is necessary. Minimum end lap should be 200mm and for roof pitches below 8º, the lap should be treated with a recommended sealant.